Research Article
Investigations of Physical and Rheological Properties of Aged Rubberised Bitumen
Table 2
The chemical components of the original bitumen before and after ageing.
| ā | Unaged | After RTFOT | After PAV |
| Saturates (%) | 15.1 | 13.88 | 12.47 | Aromatics (%) | 48.55 | 44.19 | 38.55 | Resins (%) | 26.22 | 28.94 | 31.21 | Asphaltenes (%) | 10.13 | 12.99 | 17.77 |
|
|