Mechanical Characterization of Cryomilled Al Powder Consolidated by High-Frequency Induction Heat Sintering

Figure 6

Effect of sintering time on Vickers hardness in (a) as compared to differently processed 1050 Al and percentage of full density in (b) for the powders cryomilled for 7 hours at a sintering temperature of 500°C.