Research Article

Misfit in Inconel-Type Superalloy

Figure 2

Scheme (top view) of the out-of-furnace measurement. If the sample is not -rotating in the range of 360° during the measurement, the reflection can be shifted by with respect to the expected position as it can originate from a large excentric grain. The shifts are different for different reflections as different grains scatter.
408347.fig.002