Research Article
Development and Performance Evaluation of Very High Early Strength Geopolymer for Rapid Road Repair
Table 3
Mixture formulations.
| Sample | SiO2/Al2O3 (molar ratio) | CaO/SiO2 (molar ratio) | Na2O/SiO2 (molar ratio) | H2O/Na2O (molar ratio) |
| Control | 2.77 | 0.01 | 0.21 | 11.43 | P10 | 2.85 | 0.08 | 0.23 | 11.43 | P20 | 2.95 | 0.16 | 0.25 | 11.43 | P30 | 3.09 | 0.26 | 0.27 | 11.43 | O5 | 2.88 | 0.02 | 0.22 | 11.43 | O10 | 3.01 | 0.03 | 0.22 | 11.43 | O15 | 3.15 | 0.04 | 0.22 | 11.43 |
|
|