Research Article

Evaluation of Normal and Nanolayer Composite Thermal Barrier Coatings in Fused Vanadate-Sulfate Salts at 1000°C

Figure 1

Taking care to stay within 3-4 mm from the edge, the coating surface was covered by 30 mg/cm2 of powdery mixture, forming an even film of corrosive material (in order to prevent the effects of edge corrosion).
790318.fig.001