Experimental Investigation on Material Transfer Mechanism in WEDM of Pure Titanium (Grade-2)

Figure 7

SEM micrographs of subsurface cracks at various pulse on time and peak current: (a) = 1.1 μs, Ip = 160 A, (b) = 1.1 μs, Ip = 200 A, (c) = 0.9 μs, Ip = 120 A, (d) = 0.9 μs, Ip = 160 A.
847876.fig.007a
(a)
847876.fig.007b
(b)
847876.fig.007c
(c)
847876.fig.007d
(d)

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19.