Research Article
Thermomechanical Behavior of High Performance Epoxy/Organoclay Nanocomposites
Table 2
Cure and postcure temperature peak factor and the glass transition temperature
for different epoxy systems.
| Epoxy system | Cure and postcure temperature | Peak factor () | (°C) |
| EPX_DETA | 110°C/7 h | 0.1706 | 126.5 | EPX_DDS | 160°C/5 h | 0.2878 | 175.1 | EPX_DETApc | 130°C/7 h/2 h | 0.7590 | 140.5 | EPX_DDSpc | 200°C/5 h/2 h | 0.1690 | 212.2 |
|
|