Research Article

Effects of Rolling Reduction and Strength of Composed Layers on Bond Strength of Pure Copper and Aluminium Alloy Clad Sheets Fabricated by Cold Roll Bonding

Figure 6

Results of tensile shear tests, (a) and (b) are Cu/Al-50% and Cu/Al-75%, (c) and (d) are Cu/AA5052-50% and Cu/AA5052-75%, and (e) and (f) are Cu/AA5083-50% and Cu/AA5083-75%. Left and right column represent load-displacement curves and shear stress displacement curves, respectively.
614821.fig.006a
(a)
614821.fig.006b
(b)
614821.fig.006c
(c)
614821.fig.006d
(d)
614821.fig.006e
(e)
614821.fig.006f
(f)