Research Article
The Influence of Nickel and Tin Additives on the Microstructural and Mechanical Properties of Al-Zn-Mg-Cu Alloys
Table 2
The heat treatment steps of studied alloys after the extrusion process.
| Number of treatment | Type | Details of treatment |
| 1 | Homogenizing | 450°C for 2 h + 470°C for 24 h + 480°C for 0.5 h | 2 | Peak ageing (T6) | 120°C for 24 h (peak ageing) | 3 | Retrogression and reaging (RRA) | 120°C for 24 h (peak ageing) + 180°C for 0.5 h (retrogression) + 120°C for 24 h (reageing) |
|
|