Validation results.

Sample numberRotational speed (rpm)Feed rate (mm/min)Predicted wear volume (mm3)Actual wear volume (mm3)Predicted Vickers microhardness (HV)Actual Vickers microhardness (HV)

114001500.4706820.48110444.2944.84
213001800.4258110.41295143.0542.55
310003000.3256460.33040340.0440.62
415001000.5000390.49067145.1345.03
515001500.5450250.55210746.1646.55
617001000.6585750.66219248.9449.59