Research Article
Experimental Investigation on Use of Wheat Straw Ash and Bentonite in Self-Compacting Cementitious System
Table 2
Water demand, superplasticizer demand, and setting time of SCP formulations.
| Formulation | Water demand (mass% of cement) | Superplasticizer demand (mass% of cement) |
Setting time (min) | Initial | Final |
| CEM | 28 | 0.146 | 225 | 310 | C + 10% WSA | 36 | 0.260 | 270 | 365 | C + 10% BN (H) | 33 | 0.320 | 260 | 360 | C + 10% BN (R) | 32 | 0.270 | 265 | 370 |
|
|