Experimental Investigation on Use of Wheat Straw Ash and Bentonite in Self-Compacting Cementitious System

Table 3

Variation in oxide composition of SCP formulations at 1 and 7 days.

OxidesCEMC + 10% WSAC + 10% BN (H)C + 10% BN (R)
1 day7 days1 day7 days1 day7 days1 day7 days

CaO55.8459.3558.3249.5954.2948.0655.2452.18
SiO223.168.7825.328.8729.249.5025.249.80
SO37.3417.446.7523.308.4919.757.4922.15
Al2O37.9213.437.2914.127.5915.256.8314.45
Fe2O31.283.574.521.592.801.554.401.69
K2O1.201.060.680.711.321.221.081.05
MgO2.480.401.190.561.290.522.100.62