Fabrication of Ni-Mn Microprobe Structure with Low Internal Stress and High Hardness by Employing DC Electrodeposition
Figure 8
(a) The typical probe force and contact resistance curves with respect to the overdrive stroke during cyclic testing; (b) the performances of the probe after selected number of testing cycles.