Flexural cracks against the maximum load in sample beams.
| Sample beams | Maximum load (N) | Strain gauge 4 (mm) |
| K101 | 99000 | 62 | K102 | 92600 | 68 | K103 | 95900 | 74 | KC201 | 116400 | 0.68 | KC202 | 119200 | 0.71 | KC203 | 117500 | 0.66 | KG301 | 122700 | 0.14 | KG302 | 124600 | 0.21 | KG303 | 121000 | 0.22 |
|
|