Research Article
Effect of the Aggressive Environment on the Damage of a Glass Polyester Composite Developed by Hand Layup Process
Table 2
Contents of the metal elements in the acid and alkaline solutions.
| Solutions | Elements (mg/L) | Co | Mg | Ca | Al |
| H2SO4 after 1200 hours (cont. resin) | 0,0000 | 0,1426 | 1,8542 | 0,9620 | H2SO4 after 1200 hours (cont. composite) | 0,0000 | 8,5755 | 50,2541 | 36,4050 | NaOH after 120 hours (cont. resin) | 0,0446 | 0,3600 | 1,2419 | 0,9620 | NaOH after 120 hours (cont. composite) | 0,5633 | 0,4624 | 6,8449 | 8,5569 |
|
|