Research Article
A Study on the Bond Behavior of Corroded Reinforced Concrete Containing Recycled Aggregates
Table 2
Mixtures of specimen.
| Number | w/c | Ingredients (kg/m3) | Slump (cm) | RA | NA | C | FA | KF | S | W |
| HRC1 | 0.28 | 0 | 1050 | 420 | 90 | 90 | 670 | 168 | 21.8 | HRC2 | 0.28 | 525 | 525 | 420 | 90 | 90 | 670 | 168 | 16.5 | HRC3 | 0.28 | 1050 | 0 | 420 | 90 | 90 | 670 | 168 | 9.3 | RC1 | 0.5 | 0 | 1150 | 420 | 0 | 0 | 750 | 210 | 12.0 | RC2 | 0.5 | 575 | 575 | 420 | 0 | 0 | 750 | 210 | 4.1 | RC3 | 0.5 | 1150 | 0 | 420 | 0 | 0 | 750 | 210 | 2.8 |
|
|