Research Article
Influence of Heat Treatment on Biocorrosion and Hemocompatibility of Biodegradable Mg-35Zn-3Ca Alloy
Table 1
Details of the heat treatment parameters of the Mg-35Za-3Ca alloy.
| Type of treatment | Group designation and treatment conditions | AT0 | AT1 | AT2 | AT3 | AT4 |
| Solution treatment | 310°C, 48 h | 310°C, 48 h | 310°C, 48 h | 310°C, 48 h | 310°C, 48 h | Aging treatment | Untreated | 170°C, 2.5 h | 170°C, 5.0 h | 170°C, 7.5 h | 170°C, 10 h |
|
|