DC magnetic properties of ribbons produced by melt spinning.

Thickness (mm)Magnetic flux
density (T)
Residual magnetic flux
density (T)
Relative permeabilityCoercivity (A/m)

Melt spinning
ribbon
0.031.271.381.501.121123435.65
Cold rolling
ribbon [9]
0.051.401120040.83
CVD
ribbon [4]
0.11.291.4023000