Research Article
Magnetic Properties and Core Loss Behavior of Fe-6.5wt.%Si Ribbons Prepared by Melt Spinning
Table 3
Core losses of melt spinned ribbons compared with ribbons from cold rolling and CVD.
| Method | Thickness (mm) | Core loss (W/kg) | | | | | | | | | | |
| Melt spinned | 0.03 | 7.31 | 5.47 | 1.90 | 6.99 | 1.21 | 4.62 | 3.13 | 6.03 | 10.86 | 16.69 | Cold rolled | 0.05 | 8.66 | 6.3 | — | 8.82 | — | 6.23 | — | 8.81 | 16.5 | 26.1 | CVD | 0.05 | 6.1 | 4.6 | — | 6.2 | — | 5.1 | — | 7.0 | 12.7 | 20.5 |
|
|