Improvement of Surface Properties of Inconel718 by HVOF Coating with WC-Metal Powder and by Laser Heat Treatment of the Coating

Table 2

Coating processes prepared by Taguchi program and OCP of the highest surface hardness.

ProcessOxygen
FR
Hydrogen
FR
Feed
rate
Spray
distance (in)
Hardness
(Hv)

13053256 973
23057307943
33061358913
43453357976
53457258942
63461306930
738533081033
83857356960
93861257998
OCP38532571150

FR: flow rate (FMR = 12 scfh = 9.44 10−5 m3/s), feed rate: g/min, and OCP: optimal coating process.