Research Article
On the Durability of Sealable Circular Concrete Structures under Chloride Environment
Figure 6
The evolution of chloride concentration with a sealing membrane applied at the outer surface of a concrete column, after 40 years. The surface chloride evolution and diffusivity assume the same conditions as those of Figure 4. A nominal thickness of 5 mm was reserved for the sealing membrane. m. .