Research Article
Influence of Molarity and Chemical Composition on the Development of Compressive Strength in POFA Based Geopolymer Mortar
Table 5
The percentage (%) increase in the compressive strength at 3, 7, and 14 days compared with the 28-day strength.
| Mortar designation | Increase of compressive strength (%) | 3-day (%) | 7-day (%) | 14-day (%) |
| M1 | 80 | 85 | 90 | M2 | 87 | 90 | 96 | M3 | 72 | 78 | 91 | M4 | 90 | 93 | 97 | M5 | 80 | 84 | 89 | M6 | 68 | 73 | 85 | M7 | 88 | 93 | 97 | M8 | 75 | 81 | 88 | M9 | 91 | 94 | 100 | M10 | 87 | 90 | 98 | M11 | 86 | 88 | 93 | M12 | 90 | 94 | 97 | M13 | 84 | 87 | 94 | M14 | 83 | 91 | 96 | M15 | 87 | 87 | 95 | M16 | 90 | 96 | 100 | M17 | 85 | 89 | 96 | M18 | 81 | 81 | 86 |
|
|