Hardness along the circle of 1/2 radius and center of the samples with different temperatures.
| Temperature (°C) | 760 | 800 | 840 | 880 | 920 | Average | Center | Average | Center | Average | Center | Average | Center | Average | Center |
| Hardness (HRC) | 20.08 | 19.77 | 24.36 | 23.33 | 32.78 | 29.00 | 42.44 | 41.60 | 44.29 | 43.37 | Difference (%) | 1.54 | 4.22 | 11.52 | 1.97 | 2.08 |
|
|