| Sample | Rate of the second heat emission peak (J/g·h) | Total heat emission (J/g) | 12 h | 48 h | 60 h | 72 h |
| C | 8.262 | 61.67 | 150.85 | 158.41 | 164.06 | GP-20 | 6.973 | 55.18 | 132.61 | 139.49 | 144.71 | GP-40 | 5.787 | 54.62 | 103.45 | 108.67 | 117.78 |
|
|