Research Article
Mechanical Performance versus Corrosion Damage Indicators for Corroded Steel Reinforcing Bars
Table 7
Ranges for corrosion rates related to exposure classes immediately after corrosion initiation (
) [
24].
| Exposure class | Corrosion current density [A/cm²] | Corrosion rate [m/year] |
| X0 | ≈0,01 | 0,12 | XC1 | ≈0,01 | 0,12 | XC2 | 0.1–0.5 | 1.16–5.80 | XC3 | 0.05–0.2 | 0.58–2.32 | XC4 | 0.01–0.5 | 0.12–5.80 | XD1 | 0.1–0.2 | 1.16–2.32 | XD2 | 0.1–0.5 | 1.16–5.80 | XD3 | 0.5–5.0 | 5.80–58.10 | XS1 | 0.5–5.0 | 5.80–58.10 | XS2 | 0.1–1.0 | 1.16–11.60 | XS3 | 1.0–10.0 |
11.6–1160 |
|
|