Research Article
Characterization of Waste Material Derived Willemite-Based Glass-Ceramics Doped with Erbium
Figure 1
The XRD patterns of the willemite-based glass-ceramic (Zn2SiO4) sample doped with 3 wt% Er2O3 sintered at the temperature of 500–1100°C for 4 h.