Research Article

Characterization of Waste Material Derived Willemite-Based Glass-Ceramics Doped with Erbium

Figure 2

FTIR spectra of the willemite-based glass-ceramic samples doped with 3 wt% Er2O3 sintered at the temperature of 500–1100°C for 4 h.