Feasibility of Reprocessing Natural Fiber Filled Poly(lactic acid) Composites: An In-Depth Investigation
Table 7
TGA of WF 50 PLA composite at cycle 0 and cycle 6.
| Property | Cycle 0 | Cycle 6 |
| Onset thermal degradation Temperature (°C) | 312.42 | 316.10 | Fastest decomposition Temperature (°C) | 327.06 | 337.22 | Residue (%) | 0 | 1.35 |
|
|