The Effect of Commercial Rice Husk Ash Additives on the Porosity, Mechanical Properties, and Microstructure of Alumina Ceramics

Figure 6

Distribution of the open pore size of the samples of porous alumina ceramic sintered at 1600°C for 2 hrs with different ratios of rice husk ash.