Research Article
Effectiveness of Saturated Coral Aggregate and Shrinkage Reducing Admixture on the Autogenous Shrinkage of Ultrahigh Performance Concrete
Table 2
The properties testing table of coral aggregate in China.
| Detecting items | Units | Detecting results |
| Moisture content | % | 0.2 | Organic matter | g/kg | 2.77 | Available phosphorus | mg/kg | 6.8 | pH | ā | 9.3 | Bulk density | mg/m3 | 1.37 | Texture | ā | Sand | Available nitrogen | mg/kg | 12.0 | Available potassium | mg/kg | 7.38 | Carbonate | g/kg | 987 | EC value | mS/cm | 0.140 | Total nitrogen | g/kg | 0.174 | Total phosphorus | g/kg | 0.075 | Total potassium | g/kg | 0.991 | Available boron | mg/kg | 0.201 | Cation exchange capacity | cmol/kg | 1.22 | Available copper | mg/kg | 0.218 | Available zinc | mg/kg | 0.073 | Available iron | mg/kg | 0.582 |
|
|