Research Article
Development of Electrohydraulic Forming Process for Aluminum Sheet with Sharp Edge
Table 2
FLD test conditions for this study.
| Material | A5052-H32 |
| Thickness (mm) | 0.5 | Specimen direction | Rolling direction | Temperature (°C) | 25 | Punch speed (mm/min) | 80 | Lubrication | Grease |
|
|