Time-Dependent Behavior of Shrinkage Strain for Early Age Concrete Affected by Temperature Variation
Table 3
Test parameters and results.
| Number | w/c | c (kg/m3) | Geometry (mm) | (days) | (°C) | (%) | | (days) | 0 | 1 | 3 |
| Wischers-1 | 0.48 | 325 | C 150 × 600 | 0.83 | 20 | 65 | Strain (1 × 10−6) | 0 | −25 | −42 | Wischers-2 | 0.40 | 400 | C 150 × 600 | 0.42 | 20 | 65 | 0 | −51 | −91 | Han-1 | 0.316 | 475 | P 100 × 400 | 0.67 | 20 | 50 | 0 | −115 | −189 | Han-2 | 0.316 | 475 | P 100 × 400 | 0.67 | 20 | 50 | 0 | −122 | −190 | Han-3 | 0.316 | 475 | P 100 × 400 | 0.67 | 20 | 50 | 0 | −92 | −153 |
|
|