Research Article

A Study on Insulation Characteristics of Glass Wool and Mineral Wool Coated with a Polysiloxane Agent

Table 2

Moisture absorption amount of glass wool before and after SH-AF treatment.

ClassificationWeight of the sample before SH-AF coatingWeight of the sample after SH-AF coating

Before humidification (g)4.504.38
After Humidification (g)4.894.40
Water content (g)0.390.02
Percentage of moisture content (%)8.670.46