Research Article
The Adhesion of CrN Thin Films Deposited on Modified 42CrMo4 Steel
Figure 1
Metallographic photos taken on SEM: (a) initial substrates; (b) shot-peened substrate (t = 120 s, p = 0.45 MPa); (c) shot-peened substrate (t = 360 s, p = 0.45 MPa); (d) shot-peened substrate (t = 600 s, p = 0.45 MPa).
(a) |
(b) |
(c) |
(d) |