Research Article
Effect of Reduction in Thickness and Rolling Conditions on Mechanical Properties and Microstructure of Rolled Mg-8Al-1Zn-1Ca Alloy
Figure 4
Optical micrographs and inverse pole figure maps of the AZX811 hot-rolled alloy. Total reduction ratios are as follows: (a), (d) 8.3%; (b), (e) 42%; and (c), (f) 75%.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |