Table 4

Average of mass loss of steel arising from corrosion after galvanic cell monitoring depending on the applied current density and binder type.

Binder typeMass loss (%)
Processing lossUntreated250 mA/m2500 mA/m2750 mA/m2

OPC0.230.890.550.330.30
60% GGBS0.790.480.270.27