Research Article
Development of a Semirigid Pavement Incorporating Ultrarapid Hardening Cement and Chemical Admixtures for Cement Grouts
Table 4
Flexural test results of all specimens.
| ā | Flexural strength (MPa) | Midspan deflection (mm) | Flexural strain (%) |
| Asphalt skeleton | 0.64 | 1.57 | 0.524 | PG-1 | 3.21 | 0.64 | 0.212 | SG-1 | 2.92 | 0.63 | 0.211 | FG-1 | 3.18 | 0.71 | 0.237 | FG-2 | 3.10 | 0.74 | 0.247 |
|
|