Research Article
Optimising the Performance of Cement-Based Batteries
Table 3
Cement battery designs.
| Ref. | CEM I (g) | Water (g) | Anode | Cathode | Pl (g) | CB (g) | Additive (g) or space between electrodes (mm) | Photo |
| WC 1 | 300 | 90 | Al | Cu | | | | | WC 2 | 300 | 120 | Al | Cu | | | WC 3 | 300 | 150 | Al | Cu | | | WC 4 | 300 | 180 | Al | Cu | | |
| Al 4 : 1 Cu | 900 | 360 | Al | Cu | 15 | 5 | | | Al 3 : 1 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 2 : 1 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 1 : 1 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 1 : 2 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 1 : 3 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 1 : 4 Cu | 900 | 360 | Al | Cu | 15 | 5 | Al 4 : 4 Cu | 900 | 360 | Al | Cu | 15 | 5 |
| Add 1 | 300 | 120 | Al | Cu | | | | | Add 2 | 300 | 120 | Al | Cu | | | 100 g sand | Add 3 | 300 | 120 | Al | Cu | | | 100 g agg | Add 4 | 300 | 120 | Al | Cu | 5 | | | Add 5 | 300 | 120 | Al | Cu | 5 | 5 | | Add 6 | 300 | 120 | Al | Cu | 5 | 5 | 100 g silica fume |
| Soln 1 | 300 | — | Al | Cu | 5 | 5 | 120 g 0.5 M NaCl | | Soln 2 | 300 | — | Al | Cu | 5 | 5 | 120 g 0.5 M Epsom | Soln 3 | 300 | — | Al | Cu | 5 | 5 | 120 g 0.5 M Alum | Crys 1 | 300 | 120 | Al | Cu | 5 | 5 | 100 g Epsom salt | Crys 2 | 300 | 120 | Al | Cu | 5 | 5 | 100 g Alum salt |
| SS 1 | 300 | — | Al | Cu | 5 | 5 | 120 g sodium silicate | | SS 2 | 300 | 100 | Al | Cu | 5 | 5 | 20 g sodium silicate | SS 3 | 300 | 120 | Al | Cu | 5 | 5 | Sodium silicate coating |
| Sp 1 | 300 | 120 | Al | Cu | 5 | 5 | 5 mm | | Sp 2 | 300 | 120 | Al | Cu | 5 | 5 | 10 mm | Sp 3 | 300 | 120 | Al | Cu | 5 | 5 | 30 mm | Sp 4 | 300 | 120 | Al | Cu | 5 | 5 | 60 mm | Sp 5 | 300 | 120 | Al | Cu | 5 | 5 | 80 mm |
| CB 1 | 300 | 120 | Al | Cu | 5 | 3 | | | CB 2 | 300 | 120 | Al | Cu | 5 | 4.5 | CB 3 | 300 | 120 | Al | Cu | 5 | 6 | CB 4 | 300 | 120 | Al | Cu | 5 | 7.5 |
| El 1 | 300 | 120 | Mg | Cu | 5 | 5 | | | El 2 | 300 | 120 | Al | Cu | 5 | 5 | El 3 | 300 | 120 | Zn | Cu | 5 | 5 | El 4 | 600 | 230 | Al | C | 12 | 12 |
|
|