Research Article
Effect of Solidification Rate and Rare Earth Metal Addition on the Microstructural Characteristics and Porosity Formation in A356 Alloy
Figure 14
Porosity distribution in degassed A356 alloy castings obtained from the variable angle mold heated at 350°C.