Experiment Analysis of Concrete’s Mechanical Property Deterioration Suffered Sulfate Attack and Drying-Wetting Cycles
Figure 17
The pore evolution rules of concrete specimens exposed to drying-wetting cycles with sulfate attack. (a) Initial stage, (b) filling stage, (c) expanded stage, and (d) connected stage.