Research Article
Quantitative Analysis on Force Chain of Asphalt Mixture under Haversine Loading
Table 2
Asphalt binder properties of SK 70#.
| Index | Unit | Technical requirements | Measured results |
| Penetration (25°C, 5 s, 100 g) | 0.1 mm | 60~80 | 72 | Penetration index | — | −1.5~+1.0 | −0.94 | Ductility (15°C) | cm | ≥100 | >150 | Softening point | °C | ≥46 | 48.2 | Solubility (trichloroethylene) | % | 99.5 | 99.92 | Paraffin content | % | 2.2 | 1.72 |
| Residue after thin film oven (163°C, 5 h) | Mass loss | % | ≤±0.8 | 0.1 | Penetration ratio (25°C) | % | ≥61 | 70.8 | Ductility (15°C) | cm | ≥15 | 15 |
|
|