Effect of Aluminum Addition on the Microstructure, Tensile Properties, and Fractography of Cast Mg-Based Alloys
Figure 2
Backscattered electron images showing the size and distribution of the Mg-Al-Zn phase in: (a) A alloy, 4 wt% Al; (b) C alloy, 9 wt% Al; (c) D alloy, 11 wt% Al; (d) E alloy, 14 wt% Al. Note: white particles are Mn-Al phase and gray particles are Mg-Al-Zn phase.
(a) |
(b) |
(c) |
(d) |
(e) Optical microstructure of the C alloy showing (a) Al-Mn phase and (b) Mg17(Al,Zn)12 phase; note its eutectic morphology |