Research Article

The Influence of the Activation Temperature on the Structural Properties of the Activated Carbon Xerogels and Their Electrochemical Performance

Figure 6

Cyclic voltammograms of CX and ACX electrodes at scan rates of 10 mVs−1 (a) in 1 M H2SO4; (b) in 1 M TEABF4/ACN; (c) in 6 M KOH electrolyte solutions and (d) cyclic voltammograms of ACX-900 electrode at various scan rates from 10 to 100 mVs−1.
(a)
(b)
(c)
(d)