Specific capacitance of the CX and ACX electrodes in 6 M KOH electrolyte obtained by the charge/discharge galvanostatic measurements at current densities 1 Ag−1 and 5 Ag−1.

SampleSpecific capacitance/Fg−1
1 Ag−15 Ag−1

CX159119
ACX-700178129
ACX-800186135
ACX-900204153
ACX-1000161120