Research Article
Study on the Effect of Different Fe2O3/ZrO2 Ratio on the Properties of Silicate Glass Fibers
Table 3
Tensile strength and strength retention rate of samples before and after corrosion in saturated Ca(OH)2 solution.
| Sample | 1# | 2# | 3# | 4# | E-glass | AR-glass |
| /MPa | 2936.72 | 2798.74 | 2240.21 | 1804.86 | 2340.27 | 2417.90 | /MPa | 2780.49 | 2468.69 | 1889.44 | 1338.11 | 1538.56 | 2032.74 | Strength retention rate/% | 94.68 | 88.21 | 84.34 | 74.14 | 65.74 | 84.07 |
|
|