Failure Modes in Concrete Repair Systems due to Ongoing Corrosion

Table 1

Mix proportion of SHCC mix (weight %).

CEM I 42.5NLimestone powderBlast furnace slagWater/powder ratioSuperplasticizerPVA fiber (by volume, %)

13.332.330.260.0052