Research Article
Effect of Temperature-Force Factors and Concentrator Shape on Impact Fracture Mechanisms of 17Mn1Si Steel
Table 5
Fracture micromechanisms in the crack initiation zone for specimens with different-shaped concentrators.
| Test temperature | Notch shape | V | U | I |
| | Ductile fracture with macrodimples of size 40–80 μm | Ductile fracture with macro- and microdimples | Ductile fracture with macrodimples of size ~40 μm | | Ductile fracture with macro- and microdimples | Ductile-brittle delaminations | Facet fracture, ductile-brittle fracture | | Brittle fracture with river-like fracture pattern | Ductile-brittle fracture with facets + microdimples | Brittle fracture with partial local microscopically ductile ridges |
|
|