Research Article
Corrosion Behavior of Alloy C-276 in Supercritical Water
Table 1
EDS of oxide particles and oxide films after immersion for 500 h.
| Element | Oxide particle | Oxide film |
| O | 27.51 | 25.77 | Cr | 17.69 | 23.91 | Nb | 1.51 | 2.08 | Ni | 51.73 | 46.27 | Mo | 1.56 | 1.97 |
|
|