Research Article
A Laboratory Investigation into the Effects of Coarse Aggregate Angularity on Performance of WMA
Table 4
The sieving of limestone.
| Size sieve (mm) | Passing ratio (%) | 16 | 13.2 | 9.5 | 4.75 | 2.36 | 1.18 | 0.6 | 0.3 | 0.15 | 0.075 |
| Filler | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 99.9 | 99.8 | 99.4 | 97.6 | 82.7 | 0–4.75 | 100.0 | 100.0 | 100.0 | 94.8 | 68.8 | 49.4 | 36.5 | 27.8 | 23.1 | 17.1 | 4.75–9.5 | 100.0 | 100.0 | 97.8 | 25.8 | 6.7 | 4.8 | 4.0 | 3.7 | 3.4 | 2.9 | 9.5–16.0 | 100.0 | 95.6 | 41.2 | 7.8 | 4.2 | 3.5 | 3.3 | 3.1 | 2.9 | 2.4 |
|
|