Research Article
Damage Evolution of Steel-Polypropylene Hybrid Fiber Reinforced Concrete: Experimental and Numerical Investigation
| No. | Specimens | SF | PF | (MPa) | (MPa) | Vsf (%) | lsf/dsf | Vpf (%) | lpf/dpf |
| 1 | S000P000 | — | — | — | — | 47.53 | 2.75 | 3 | SB15P000 | 1.50 | 60 | — | — | 52.91 | 4.47 | 4 | S000P15 | — | — | 0.15 | 167 | 48.80 | 3.47 | 7 | SB10PA15 | 1.00 | 60 | 0.15 | 167 | 55.2 | 4.13 | 8 | SB15PA10 | 1.50 | 60 | 0.10 | 167 | 58.05 | 4.61 | 9 | SA15PA15 | 1.50 | 30 | 0.15 | 167 | 54.65 | 4.19 | 10 | SB15PA15 | 1.50 | 60 | 0.15 | 167 | 53.35 | 4.25 | 13 | SC15PA15 | 1.50 | 80 | 0.15 | 167 | 53.70 | 4.76 | 14 | SB15PA20 | 1.50 | 60 | 0.20 | 167 | 50.91 | 3.76 | 15 | SB20PA15 | 2.00 | 60 | 0.15 | 167 | 56.22 | 5.36 |
|
|